There is a fusing and kiln formed section in the gallery but not on this message board. Unless I am missing something. It would be great to have a fusers section. Lisa
What's up Lisa? There seems to be a shortage of fusers here. Great to see you here.
I haven't fused any soft glass in a while, but I'll probably start again after a tour of Bullseye.
Is there a particular topic you'd like to open up?
Tin-side? Dichro on soft glass? (WHA?) Borax? Enamels? Thompson? Satellite? Fusemaster? 7-up as mixing media? What are all these crazy ideas? Jump in and find out! We'd love to discuss these topics and anything else we can learn from YOU! Peace, Fred.
hey Fred, Used baking soda once and the bubbles took me away. There is a limit to everything. Just bought a wonder ful SS mold 41/2" dia. by 4 deep, pyramid shape for paper weights. Won't fill up the whole mold and then maybe I will....... Working with thicker suff to cut up and add to pieces.never ends. just got in and I have to eat and run out again. Glad you replied. Lisa